Looking at the precautions when using furniture paper?

Your current position: Home page >> News >> Lndustry news

Looking at the precautions when using furniture paper?

Date of release:2018-05-22 Author: Click:

Furniture paper can change the shape of the furniture. If there are wrinkles in the process of posting, it will affect the overall furniture decoration effect, and need to be torn off and restart. If you want to avoid wrinkles, you should prepare well before posting. Under normal circumstances, the substrate used as a sticker is mostly wood chipboard. If you directly apply stickers on the surface of these two kinds of plates, you will often see stickers. The problem of unevenness means that the substrate must be treated to make it smooth.

Furniture Paper: As the name implies, furniture paper is made of wood-textured veneer as a substrate for furniture. Wood grain veneer is different from solid wood and veneer veneer, but it has the effect of wood grain. In general, paint stickers should focus on the following aspects:

First, the processing of the substrate: Under normal circumstances, the substrate used as a sticker is mostly a particle board, and if the sticker is directly on the surface of the two plates, the problem of unevenness tends to occur, so the base must be The material is processed to make it smooth and smooth. For example, full of water ash on the sheet, scrape putty, spray PU or PE solid color primer and so on. The advantage of full batch of water ash is its low cost, and its disadvantage is mainly the problem of adhesion. Although the putty solves the problem of adhesion to the substrate, we know that the putty on the market is mostly a one-component nitro putty, and from the matching of the paint, it is easy to cause between the upper polyester and the thinner. The bottoming phenomenon that occurs when the reaction occurs. Spraying a PU or PE solid color primer will not cause the above problems. Therefore, it is also the most popular at present.


7.png


Second, the choice of paint: the effect of sticker furniture is good or bad, the first is to look at its transparency, followed by color, fullness, hardness, feel and so on. If the transparency of the paint is not good, it will directly affect the clarity and look of the color. Therefore, choosing the paint with good transparency is the most important. For example, the primer, we can choose China Resources' PU type PD3900, PD3300, PD3600, and PD1500 transparent primer and PE type ED3100, ED3300, ED3600 and ED3900 transparent primer, etc., achieve high transparency and good filling force. , fullness, hardness, resistance to yellowing, abrasion and other effects. Topcoats, we can choose China Resources's PU class P3600X, P3800X, P3400X and P2800X and PE class ED3000, which not only guarantees good transparency, but also can meet the paint film hardness, scratch resistance, fullness, feel, resistance to yellow Change and other requirements.

Third, the painting process: the quality of the furniture, the effect, not only depends on the quality of the board. The quality of the paint, and the selection of a reasonable coating process is also very important. In general, the process of painting sticker furniture can be divided into the following processes:

1. White billet processing. Grind with 240#—320# sandpaper to eliminate surface stains and make the surface smooth.

2. Closed. Closed with the China Resources PS900 Depot, polished after 3-4 hours.

3. Polishing. Lightly grind with 320# sandpaper to remove wood thorns.

4, the primer. Spray Huarun PU or PE solid color primer to achieve a certain fullness and hiding power. Do not leak the bottom and polish it after 5-8 hours.

5, polished. Sanding with 320# sandpaper is smooth and smooth.

6, stickers. With wood-grain paper, the sticker requires no bubbles, no wrinkles, neat and consistent, and after 24 hours of drying, the primer is applied.

7, primer. Spray Huarun PU or PE transparent primer to achieve a certain fullness, and sand it after 5-8 hours.

8, polished. Smooth and smooth with 400#-600#, require no obvious sand marks, no bright spots.

9, repair color. The Huarunshi Na or the color essence and the clear top coat are proportioned and sprayed, and the color is required to be uniform, and the sand is polished after 8-10 hours.

10. Polish. Lightly grind with 800#—1000# sandpaper to remove surface particles.

11, cover light. With China Resources Clear Coat, spray, require filtration, pay attention to dust, and work hard after 24 hours.

The quality of the furniture paper is good and bad quality is always a point, transparency, color, fullness, hardness, feel, etc. all affect its fried ug you love Oh, with good materials after using the appropriate process There will be different effects. The quality of the furniture, and how effective it is, depends not only on the quality of the sheet. The quality of the paint, and the selection of a reasonable coating process is also very important.